Exterior wall rock wool board features weak peel resistance. Its thermal conductivity stands at 0.03~0.047W/(m·K) under 25℃ ambient temperature.
Rock wool and slag wool are non-combustible inorganic silicate fibers. Flammable binders added during manufacturing will affect the overall fire performance.
Porous structure generates airflow resistance. Sound energy is consumed via friction, effectively blocking sound transmission.
Rock wool fiber poses lower hazard than asbestos yet shares similar biological characteristics. Core prevention methods:
Ventilation & dust removal: Install local exhaust facilities to discharge fiber dust
Wet operation: Sprinkle water in advance to cut dust generation
Personal protection: Wear dust-proof gear when necessary
Three mainstream production techniques bring distinct physical differences:
Settling MethodFibers distribute horizontally with uneven density and binder. Low peel strength, compression strength below 20kPa. High water absorption, hard to drain moisture thoroughly.
Pendulum MethodLayered stacking forms partial vertical fiber layout. Peel strength>14kPa, compression strength>40kPa. Moderate water absorption. Low thermal conductivity ≤0.036W/(m·K) at 10℃, moisture absorption<1.0%, hydrophobic rate≥98%.
3D Forming MethodFibers form three-dimensional structure, anti-delamination and anti-peeling. Peel strength>22kPa, compression strength>60kPa. Water absorption close to polystyrene board with excellent hydrophobicity. Low thermal conductivity, stable moisture resistance.